How Do Moisture Regain and Commercial Weight Work in Yarn Trade?
Product News

How Do Moisture Regain and Commercial Weight Work in Yarn Trade?

2026-10-14

100% baby cashmere yarn on cone — reference product image supplied by Consinee Group

Yarn Trade & Contract Specification

How Do Moisture Regain and Commercial Weight Work in Yarn Trade?

A buyer's calculator and a seller's contract clause: how moisture regain and commercial weight actually settle yarn invoicing, with worked cashmere examples, ASTM D1909 / ISO 6741-1 / GB/T 9995 reference values, and the 5-step moisture-clause specification protocol.

— 100% Baby Cashmere Yarn on cone — the type of yarn whose commercial weight is settled by the moisture regain convention in the contract.

100% baby cashmere yarn on cone — reference product image supplied by Consinee Group for moisture regain and commercial weight discussion
Figure 1 — 100% baby cashmere yarn on cone, supplied by Consinee Group. A cone of this yarn is sold by commercial weight, not by the scale weight at the moment of delivery. The commercial weight is the oven-dry weight multiplied by 1 plus the standard moisture regain named in the contract. For cashmere under GB/T 9995 that factor is 1.15; under ASTM D1909 it is 1.136. Browse the Consinee wholesale yarn collections →

What Are Moisture Regain and Commercial Weight, and Why Do They Run Every Yarn Contract?

Standard moisture regain is a fixed reference value, set by a national or industry standard, that defines how much water a fibre is assumed to hold for invoicing purposes. Commercial weight is the invoiced weight of a yarn or fibre lot, calculated from the oven-dry weight by applying the standard regain. The two terms together are the invisible engine of every yarn PO between a Chinese spinner and an overseas brand, and they are the most common source of contract dispute we see in 25+ years of running an export desk. The four conventions that govern these values worldwide are ISO 6741-1 (international commercial mass, iso.org/standard/65177.html), ASTM D1909 (US commercial moisture regain table, astm.org/d1909), the IWTO clean-wool basis for wool trade (iwto.org), and GB/T 9995 (Chinese national standard, openstd.samr.gov.cn).

Direct answer: Standard moisture regain is a contractual convention (a fixed number set by ASTM D1909, ISO 6741-1, GB/T 9995, or IWTO) that defines how much water a fibre is assumed to hold for invoicing. Commercial weight is the oven-dry weight multiplied by 1 plus that regain. The contract is settled on commercial weight, not on the actual scale weight at the moment the lot crosses the dock.

Two terms that look like measurements, but are actually conventions. The standard moisture regain for a given fibre is set by the standard body, not by a measurement on the actual lot. Cashmere under GB/T 9995 carries 15% standard regain. Cashmere under ASTM D1909 carries 13.6% standard regain. Both are valid. The choice is contract-driven, not measurement-driven, and the contract must name the convention in writing.

Why does this matter? Because the actual moisture content of a fibre lot at the moment of delivery depends on the warehouse, the weather, the packaging, and the transit time. A 1,000 kg shipment of 100% cashmere yarn cones can arrive at a 12% actual moisture content on a dry winter day, or at a 19% actual moisture content on a humid summer day. The commercial weight, set by the contract, holds the line at 1,150 kg under GB/T 9995 or 1,136 kg under ASTM D1909. The actual scale weight moves; the commercial weight does not. Because the actual moisture content is not a stable reference, therefore the trade has standardised on a fixed reference — the standard moisture regain — and the contract binds the parties to that fixed number.

This is the convention that runs every yarn PO, and it is also the convention that surfaces as a dispute when the spec is loose.

How to Read a Standard Moisture Regain Table Without Misquoting It

Direct answer: Read a standard moisture regain table by fibre, then by convention. ASTM D1909, ISO 6741-1, GB/T 9995, and IWTO do not always agree on the same number for the same fibre. The contract binds to one convention; the table is reference only.

Reference table — standard commercial moisture regain, by fibre and convention, per ASTM D1909 (astm.org/d1909), GB/T 9995 (openstd.samr.gov.cn), and the IWTO clean-wool basis (iwto.org):

Standard commercial moisture regain by fibre and convention (ASTM D1909 / GB/T 9995 / IWTO)
Fibre ASTM D1909 GB/T 9995 IWTO clean wool basis Notes
Cotton 8.5% 8.5% — Agreement between ASTM and GB/T
Wool (merino) 13.6% 15% 17% Three different values; convention-dependent
Cashmere 13.6% 15% — ASTM and GB/T differ
Mohair 14% 14% — Agreement
Alpaca 14% 14% — Agreement
Silk 11% 11% — Agreement
Linen (flax) 12% 12% — Agreement
Viscose / rayon 13% 13% — Agreement
Acrylic 2% 2% — Very low regain — closer to bone-dry
Polyester 0.4% 0.4% — Effectively bone-dry
Nylon 4.5% 4.5% — Low regain

Read the table by column, not by row. A buyer who quotes "15% cashmere regain" and a seller who quotes "13.6% cashmere regain" are both correct — they are quoting two different conventions. The dispute comes when the contract does not name which one applies. Three traps to watch for.

Trap 1: the spec quotes a regain percentage without naming the convention. The percentage alone is ambiguous. Fix: write the convention and the percentage in the same line, e.g. "Standard regain: 15% per GB/T 9995."

Trap 2: the spec quotes a value that does not exist in any current convention. Cashmere at "10% regain" or wool at "20% regain" is not a recognised standard — it is a custom figure, and it must be justified in writing. Because a non-standard figure is a custom value, therefore it must be agreed in writing, not assumed.

Trap 3: the spec quotes a percentage but applies the wrong formula. Some buyers and sellers treat the standard regain as if it were a percentage of the total (wet) weight, which is moisture content, not regain. The relationship is regain = moisture content / (1 - moisture content). A 15% regain corresponds to 13.04% moisture content, not to 15% moisture content. The contract formula must use the regain, not the moisture content.

Commercial Weight vs. Net Weight vs. Bone-Dry Weight — A Worked Example in Cashmere

Three weights appear in a yarn invoice. Knowing which is which is the entire game.

  • Bone-dry weight (also called oven-dry weight): the weight of the fibre after all moisture has been driven off in an oven at 105-110°C to constant mass. This is the only physically measurable, stable reference weight.
  • Net weight (also called actual weight, scale weight, gross-netting-tare weight): the weight of the fibre on the scale at the moment of weighing. This number moves with the weather, the warehouse, and the transit conditions.
  • Commercial weight (also called legal weight, invoiced weight): the bone-dry weight multiplied by 1 plus the standard moisture regain. This is the contract weight.
Direct answer: Commercial weight = bone-dry weight × (1 + standard regain). The contract settles on commercial weight, not on the scale weight at delivery. A worked cashmere example is below.

Worked example — 1,000 kg of 100% cashmere yarn, per GB/T 9995 (openstd.samr.gov.cn):

  • Lab oven-dry test: 1,000 kg of yarn, oven at 105°C to constant mass, measures 869.6 kg oven-dry weight.
  • Standard regain: 15% per GB/T 9995.
  • Commercial weight: 869.6 kg × 1.15 = 1,000 kg. The invoice is for 1,000 kg at the contract price.

If the same lot is re-tested under ASTM D1909 at 13.6% standard regain, the commercial weight is 869.6 kg × 1.136 = 987.7 kg. The oven-dry weight is identical; the standard regain is the only variable, and the convention is the only difference. A 12.3 kg delta on a 1,000 kg lot is small in percentage terms but real in dispute-resolution terms, which is why the contract must name the convention.

Worked example — the same 1,000 kg lot arriving at a different actual moisture content:

  • Bone-dry weight: 869.6 kg (unchanged; the fibre did not lose any mass during transit).
  • Scale weight on arrival: 950 kg (12% actual moisture content — arrived dry).
  • Commercial weight under GB/T 9995: still 1,000 kg. The contract is settled on commercial weight, not on the 950 kg scale weight.

This is the second trap: a buyer who pays on scale weight and signs without a commercial-weight clause pays for less yarn than the contract. A seller who delivers without a commercial-weight clause bears the weather risk on the way to the dock. The clause is the contract.

4 Trade-Dispute Scenarios That Trace Back to a Missing Moisture Clause

The single most expensive mistake on a yarn PO is not the choice of fibre, the count, or the gauge. It is omitting the standard moisture regain convention from the contract, so the invoice weight is unanchored when the lot arrives at a different actual moisture content than the invoice assumed. Four scenarios recur.

Scenario 1 — Different regain conventions on the buyer's PO and the seller's invoice

The buyer's PO quotes "15% cashmere regain" with no convention. The seller's invoice computes commercial weight at 13.6% per ASTM D1909 (the seller's house standard). The numerical difference is small per kg, but the cumulative effect on a 5,000 kg PO is real money and a real dispute. Fix: name the convention and the percentage in the same line of the PO.

Scenario 2 — Different conditioning atmospheres between seller lab and buyer lab

The seller lab conditions at 20°C / 65% RH per ISO 139. The buyer lab conditions at 23°C / 50% RH per a different internal SOP. The oven-dry weights are identical; the conditioned weights differ, and so do the regain values calculated from them. Both labs are "right" by their own convention. The dispute is unresolvable without a single named conditioning atmosphere in the contract. Fix: name ISO 139 / ASTM D1776 in the contract.

Scenario 3 — Scale weight on arrival diverges from invoice weight

The invoice says 5,000 kg commercial weight. The scale on arrival says 4,750 kg. The buyer suspects underweight. The seller suspects the buyer's scale or the buyer's conditioning room. Without a contract clause that names the conditioning standard and the retest protocol, the dispute goes to lawyers. Fix: name the retest lab (SGS, Intertek, Bureau Veritas) and the tolerance band in the contract.

Scenario 4 — Blended yarn invoice applied to wrong fibre's regain

A 70/30 cashmere/wool blend is invoiced as 100% cashmere regain. The commercial weight is overstated. The blend ratio is in the spec, but the regain convention is not, and the seller's invoicing software defaults to the dominant fibre's regain. Fix: write the regain convention for the blend, or specify a weighted-average regain. Because the convention is applied to the wrong fibre, therefore the commercial weight is misstated by an amount that the contract cannot resolve without a written formula.

How Lab Conditioning (ISO 139 / ASTM D1776) Locks the Number You Actually Trade On

The actual moisture content of a fibre is not a fixed property. It moves with the temperature and humidity of the air around it. That is why the trade has standardised on a single conditioning atmosphere, and that is why the conditioning atmosphere is named in the contract, not in the test report's footnote.

Direct answer: Standard conditioning is 20°C and 65% RH per ISO 139 and ASTM D1776. A lab that conditions at a different atmosphere produces a regain number that is not directly comparable to the contract standard. The conditioning atmosphere must be named in the contract.

The conditioning cycle is mechanical and verifiable. Samples are placed in a controlled atmosphere of 20°C and 65% RH per ISO 139, typically for 24 hours or until the mass change between two consecutive weighings is below 0.1% over a 2-hour interval. The conditioned mass is the test mass for the contract. The oven-dry mass is the test mass for the standard regain formula. The two together produce the measured regain for the lot, and the standard regain for the contract.

Two conditioning atmospheres are in use. ISO 139 specifies 20°C and 65% RH; this is the dominant atmosphere in international textile trade. ASTM D1776 specifies the same atmosphere for textile conditioning in the United States. A small number of European buyers condition at 23°C and 50% RH, which is a different reference state and produces a different measured regain. The contract must name the atmosphere or the lab will condition to the wrong standard.

The oven-dry method is the second controlled step. ASTM D2654 specifies drying at 105-110°C to constant mass. ISO 6741-1 Annex A gives the equivalent method for textile fibres and yarns. Constant mass is defined as two consecutive weighings within 0.05% over a 15-minute interval. The bone-dry mass is the reference for the standard regain formula.

5-Step Specification Protocol for a Moisture-Clause Yarn Contract

The following protocol is what we use to write or review the moisture and commercial-weight clause on an export yarn contract. Each step is a precondition for the next.

Direct answer: The five steps are (1) name the standard moisture regain convention with a percentage value, (2) name the conditioning atmosphere per ISO 139 / ASTM D1776, (3) name the oven-dry method per ASTM D2654 or ISO 6741-1 Annex A, (4) write the commercial weight formula explicitly, (5) name the dispute-resolution lab and the tolerance band. Skipping any one of the five is the most common cause of moisture-clause disputes.

Step 1 — Name the standard moisture regain convention

Pick the convention that governs the invoice: ASTM D1909, ISO 6741-1, GB/T 9995, or IWTO clean wool basis. Write the value as a percentage in the contract. For cashmere under GB/T 9995, the line is "Standard moisture regain: 15% per GB/T 9995." For wool under IWTO, the line is "Standard moisture regain: 17% on the clean wool basis per IWTO."

Step 2 — Define the laboratory conditioning atmosphere

Set the conditioning atmosphere per ISO 139 (20°C / 65% RH) and ASTM D1776. Conditioning time, sample size, and weighing precision must be in the contract, not a footnote. A typical line is "Conditioning: 20°C / 65% RH, 24 hours minimum, to constant mass per ISO 139."

Step 3 — State the oven-dry test method

Name the oven-dry method: ASTM D2654 (oven at 105-110°C to constant weight) or ISO 6741-1 Annex A. State the drying time and the constant-weight criterion. A typical line is "Oven-dry method: ASTM D2654, 105°C to constant mass (two consecutive weighings within 0.05% over 15 minutes)."

Step 4 — Lock the commercial weight formula

Write the formula explicitly: commercial weight = oven-dry weight × (1 + standard regain). For cashmere at 15% regain, 100 kg of oven-dry fibre is invoiced as 115 kg of commercial weight. A typical line is "Commercial weight = bone-dry weight × 1.15. Bone-dry weight is the oven-dry mass determined per Step 3."

Step 5 — Define the dispute-resolution protocol

State the independent lab for retest in case of dispute (SGS, Intertek, Bureau Veritas), the retest cost responsibility, and the tolerance band allowed between the seller-lab and buyer-lab results. A typical line is "Dispute resolution: retest by SGS Shanghai, cost split equally, tolerance band 0.3 percentage points of standard regain."

What to Ask a Yarn Supplier Before You Sign a Moisture-Sensitive PO

Five questions that catch 80% of the moisture-clause issues before a purchase order is committed.

Direct answer: Five questions for the supplier before PO: (1) which standard moisture regain convention is named in the contract, (2) which conditioning atmosphere does the seller lab use, (3) which oven-dry method does the seller lab use, (4) can the seller provide a per-lot commercial-weight calculation worksheet, (5) what is the dispute-resolution lab if the buyer-lab result disagrees.
  1. Which standard moisture regain convention is named in the contract? ASTM D1909, ISO 6741-1, GB/T 9995, or IWTO. The answer must be specific.
  2. Which conditioning atmosphere does the seller lab use? 20°C / 65% RH (ISO 139) or 23°C / 50% RH. The answer must be specific.
  3. Which oven-dry method does the seller lab use? ASTM D2654 or ISO 6741-1 Annex A. The answer must be specific.
  4. Can the seller provide a per-lot commercial-weight calculation worksheet? A reputable supplier provides a worksheet showing the bone-dry weight, the standard regain applied, and the commercial weight per lot. The worksheet is the auditable record.
  5. What is the dispute-resolution lab if the buyer-lab result disagrees? SGS, Intertek, or Bureau Veritas. The answer must be a named lab, not "we will work it out."

One last thing: ask for a sample shipment before committing to a 40-foot container. Every legitimate yarn supplier will agree to a sample cone or a sample carton with batch documentation, including the commercial-weight worksheet for the sample. The cost of the sample is in the noise of the cost of a misfit container.

Bringing It Together — A Buyer's Calculator and a Seller's Contract Clause

Putting the protocol into a single calculator and a single contract clause makes it easier to keep on a clipboard during a phone call with the supplier.

Buyer's calculator (5 lines, drop into a spreadsheet):

  1. Bone-dry weight (kg): from the seller lab oven-dry result.
  2. Standard regain (%): from the contract (e.g. 15% for cashmere under GB/T 9995).
  3. Commercial weight (kg) = bone-dry weight × (1 + standard regain/100).
  4. Unit price (per kg of commercial weight, in the contract currency).
  5. Invoice amount (commercial weight × unit price).

Seller's contract clause (5 sentences, drop into the PO):

  1. Standard moisture regain: 15% per GB/T 9995 (or named convention).
  2. Conditioning: 20°C / 65% RH per ISO 139, 24 hours minimum to constant mass.
  3. Oven-dry method: ASTM D2654, 105°C to constant mass.
  4. Commercial weight = bone-dry weight × 1.15. Bone-dry weight is determined per the oven-dry method above.
  5. Dispute resolution: retest by SGS Shanghai, cost split equally, tolerance band 0.3 percentage points of standard regain.

Walk through these ten lines and the moisture-clause spec lands. Anything that cannot answer one of the ten is not a complete spec.

Conclusion — Why a Tight Moisture Clause Is Cheaper Than a Loose One

Moisture regain and commercial weight are the invisible engine of every yarn PO. The convention is fixed; the actual moisture content of a lot is not. The contract binds the parties to the convention, and the convention is what the invoice is settled on.

We have walked through what we do at Consinee Group — 10,000+ tons of yarn per year, 3,000+ tons of 100% cashmere (about 20% of global cashmere output), GCS, GOTS, and GRS certified, supplying elite brands including Max Mara, Ralph Lauren, and Lululemon. The cashmere export desk runs on the moisture-clause spec above, and we open up the worksheet to buyers and procurement engineers on request.

If you are writing a yarn contract, or a yarn PO, or a yarn tender, the moisture-clause spec above is the operationally honest way to anchor the invoice weight. Send us your fibre, your count, your gauge, and your destination port, and the export desk will come back with a draft moisture-clause spec and a sample commercial-weight worksheet within 24 hours.

Frequently Asked Questions

What is the standard moisture regain for cashmere?

Cashmere carries a 13.6% standard moisture regain under ASTM D1909 and a 15% standard moisture regain under GB/T 9995 (the Chinese national standard). Both values are valid in international trade; the contract must name the convention being used so the invoice weight is anchored.

What is commercial weight in yarn trade?

Commercial weight is the invoiced weight of a yarn or fibre lot, calculated as the oven-dry weight multiplied by 1 plus the standard moisture regain. For cashmere under GB/T 9995, 100 kg of oven-dry fibre is invoiced as 115 kg of commercial weight. Commercial weight is what the contract is settled on, not the actual scale weight at delivery.

Is moisture regain the same as moisture content?

No. Moisture content is the mass of water as a percentage of the total (wet) mass of the fibre. Moisture regain is the mass of water as a percentage of the oven-dry mass. The relationship is: regain = moisture content / (1 - moisture content). The trade convention uses regain; the lab test typically measures moisture content and converts.

What is the ISO standard for commercial mass of yarn?

ISO 6741-1 (Textiles — Fibres and yarns — Determination of commercial mass) is the international standard. It pairs with ISO 139 for the standard conditioning atmosphere (20°C / 65% RH) and ASTM D2654 / ISO 6741-1 Annex A for the oven-dry test method.

Why does the same fibre have different standard regain values?

Different national and industry conventions have set different round-number reference values for the same fibre. ASTM D1909, ISO 6741-1, GB/T 9995, and the IWTO clean-wool basis do not always agree. The contract must name one convention, otherwise the invoice is ambiguous.

What is the standard regain for wool, silk, cotton, and synthetics?

Under ASTM D1909: cotton 8.5%, wool (merino) 13.6%, silk 11%, linen 12%, viscose 13%, acrylic 2%, polyester 0.4%, nylon 4.5%. Under IWTO, wool carries a 17% clean-wool-basis regain. Cashmere is 13.6% under ASTM D1909 and 15% under GB/T 9995.

What is the standard conditioning atmosphere for textile moisture testing?

ISO 139 and ASTM D1776 specify 20°C and 65% relative humidity as the standard atmosphere for conditioning and testing textile fibres and yarns. Samples are typically conditioned for 24 hours or until constant mass is reached.

How is commercial weight calculated?

Commercial weight equals oven-dry weight multiplied by 1 plus the standard moisture regain. Example: 1,000 kg of cashmere at 15% GB/T 9995 regain = 1,000 kg oven-dry × 1.15 = 1,150 kg commercial weight. The same 1,000 kg oven-dry at 13.6% ASTM D1909 regain = 1,136 kg commercial weight.

Why is commercial weight a convention rather than a measurement?

Because the actual moisture content of a fibre lot at any given moment depends on the warehouse, the weather, and the packaging. The standard moisture regain is a fixed reference value set by the standard body, and the contract binds the parties to that fixed value, so invoicing does not move with the weather.

What should I include in the moisture clause of a yarn contract?

Five items: (1) the standard moisture regain convention with a percentage value, (2) the conditioning atmosphere per ISO 139 / ASTM D1776, (3) the oven-dry method per ASTM D2654 or ISO 6741-1 Annex A, (4) the commercial weight formula written out, (5) the dispute-resolution protocol with named retest lab and tolerance band.

Send Your Spec — Get a Free Moisture-Clause Review

If you are writing a yarn contract, a yarn PO, or a yarn tender, send us your fibre, your count, your gauge, and your destination port. Our export desk will come back with a draft moisture-clause spec and a sample commercial-weight worksheet within 24 hours. Discuss commercial weight terms with the Consinee team →

Discuss commercial weight terms with the export desk →

Next Step · Free Review

Send Your Spec — Get a Free Moisture-Clause Review

If you are writing a yarn contract, a yarn PO, or a yarn tender, send us your fibre, your count, your gauge, and your destination port. Our export desk will come back with a draft moisture-clause spec and a sample commercial-weight worksheet within 24 hours.

Discuss commercial weight terms Browse wholesale yarn collections

Last verified: 2026-10-14 · Published on Consinee Top Blog